Palladium

[MIL-P-45209B]

Back | Home


Minimum thickness shall be .000050" unless otherwise specified. A gray, dense deposit; good for undercoats. Good wear characteristics, corrosion resistance and catalytic properties. Good conductivity. Steel springs and other steel parts subject to flexure or repeated impact and of hardness greater than Rc 40 shall be baked at 375°F ± 25° for three(3) hours minimum after plating.